Thermal cycling and thermal ageing tests were performed on Crofer22APU/glass-ceramic/Anode-Supported-Electrolyte (ASE) joined samples in air at the SOFC operating temperature of 800 degrees C. The Crofer22APU had been polished and preoxidised at 900 degrees C for 2 h. The diffusion behaviour at the two interfaces was examined and revealed slight diffusion of chromium and manganese from Crofer22APU into the glass-ceramic. No interactions, failure or crack formation were observed at the Crofer22APU/glass-ceramic interface and between the glass-ceramic and YSZ.

visibility_off picture_as_pdf

picture_as_pdf
AC_ALT_2.pdf
subject
Published Version
lock
Restricted to Repository staff only

Request Copy

Atom BibTeX OpenURL ContextObject in Span OpenURL ContextObject Dublin Core MPEG-21 DIDL EndNote HTML Citation METS MODS RIOXX2 XML Reference Manager Refer ASCII Citation
Export

Downloads